Design pressure |
Material | Hardness |
| 0.3–0.8MPa | HT200 or HT250 or HT300 |
HB180–HB240 |
|
Face Length |
Operating Speed | Roughness |
|
1450–6000mm |
200–600m/min |
0.4~0.2µ |
| Wall Thickness | Ingredient |
Structural Style |
|
Consult |
Alloy dryer or normal |
3 parts or 5 parts |